"First, natural wood blocks were immersed in a boiling aqueous solution of mixed 2.5 M NaOH and 0.4 M Na2SO3 for 7 h, followed by immersion in boiling deionized water several times to remove the chemicals. Next, the wood blocks were pressed at 100 °C under a pressure of about 5 MPa for about 1 day to obtain the densified wood"
"First, natural wood blocks were immersed in a boiling aqueous solution of mixed 2.5 M NaOH and 0.4 M Na2SO3 for 7 h, followed by immersion in boiling deionized water several times to remove the chemicals. Next, the wood blocks were pressed at 100 °C under a pressure of about 5 MPa for about 1 day to obtain the densified wood"
Pretty simple and straightforward.